Inline Viscosity Control in Asphalt Manufacturing

Bitumen blowing unit with inline viscosity measurement

What is Asphalt?

Bitumen, the raw material for asphalt, is a residue from the distillation of crude oil. In its natural state or after simple distillation, the mechanical properties of bitumen are limiting some industrial application. Indeed, bitumen may be very sensitivity to temperature fluctuations which affects Asphalt manufacturing or use. Air blowing alters bitumen to suit roofing, waterproofing and industrial coating applications. Viscosity measurement is one of the key parameters to determine the end point of a batch’s production. Continuous inline viscosity measurement correlates with traditional methods, such as the sampled, discrete softening-point test.

How air blowing changes Bitumen Viscosity ?

The Oxidation process involves passing a stream of hot air through the heated bitumen. Heat (230–280 °C / 440–550 °F) and oxygen trigger several simultaneous chemical reactions:

Dehydrogenation: Hydrocarbon molecules lose hydrogen atoms, promoting the formation of stronger carbon-carbon bonds.

Condensation and Polymerization: The molecules form longer, more complex structures, increasing the average polymer size.

Increase in Asphaltene Content: The heaviest and most rigid fraction of bitumen (asphaltenes) increases at the expense of maltenes, which are lighter compounds. It is this shift in balance that hardens the final product.

The result is what is known as “blown” bitumen: it is harder and less likely to soften at high temperatures, but also more brittle at low temperatures than conventional road bitumen. During this oxidation stage, the softening point and viscosity increase over time.

The Industrial Bitumen Blowing Process

1. Load preparation

Distillation bitumen, known as “straight-run” bitumen, is the raw material. It is preheated in heat exchangers until it reaches a viscosity low enough to be pumped and processed efficiently. The inlet temperature of the reactor is generally between 220 °C [446°F] and 260 °C [500°F].

2. The blower reactor

At the heart of the system is a vertical cylindrical column, the blower (or oxidizer). Compressed air is injected into the bottom of the column via a sparger, which finely disperses hot air bubbles throughout the bitumen mass. This intensive aeration promotes contact between oxygen and bitumen, thereby maximizing oxidation reactions.

The blowing time, temperature, and air flow rate are the three key parameters that determine the final grade of the product. Longer or more intense blowing produces harder bitumen with a higher softening point and lower penetration.

3. Cooling and processing

Upon exiting the reactor, the oxidized bitumen is still liquid and very hot. It is cooled, then stored in heated tanks or packaged in blocks or drums.

Quality Control: From Softening Point to Inline Viscosity

Sampling vs continuous – Quality

Historically, quality control for a batch of Asphalt was performed through sampling using one of the following standardized methods:

Penetration (ASTM D5-06) Measures the penetration depth of a standard needle into asphalt at 25 °C under a load of 100 g for 5 seconds. It is expressed in tenths of a millimeter (1/10 mm). The lower the value, the harder the asphalt.

The Softening Point (ASTM D36-95) corresponds to the temperature at which the asphalt, supporting a 3.5-gram steel ball, softens enough for the ball to fall 25 mm. A high softening point indicates good heat resistance.

Online measurement, using a sensor installed directly on the blower, reduces the number of samples taken and the need for laboratory analysis, while providing an instantaneous and continuous reading of the physical quantity being measured.

Viscosity & correlation: Bitumen & Asphalt application

Viscosity refers to a fluid’s resistance to flow: the higher the viscosity, the stiffer the material and the more resistant it is to deformation. Penetrability and viscosity are two fundamental rheological properties of asphalt that are inversely related and closely linked.

The in-line viscometer is the process sensor that plays a key role in continuous quality control during asphalt production.  

A direct correlation between the softening point measurement and the penetrability measurement is possible. The viscosity measurement performed with the MIVI under process conditions can be supplemented by a temperature-compensated viscosity (TCV) determination at a reference temperature. The approach of combining TCV with a correlation is the subject of the following blog article: TCV & Correlation: the key to process control

Main Applications

Oxidized asphalt differs from standard road bitumen in its uses:

  • Roof waterproofing: bituminous membranes, roofing felt, asphalt shingles
  • Pipeline insulation and coating: corrosion protection
  • Bituminous cardboard and bituminous kraft paper: industrial packaging
  • Seals and sealants: civil engineering applications (bridges, dams)
  • Record and electronics industry (historically): acoustic and electrical insulation

However, oxidization process is not suitable for road asphalt mixtures, for which conventional road bitumen is preferred because oxidation makes the material too brittle in cold weather and prone to cracking under traffic loads.

Toward Continuous Optimization of the Asphalt Manufacturing Process

Asphalt production presents several challenges, and online viscosity measurement has proven to be a solution that enables processes to be optimized efficiently and consistently.

The in-line viscometer plays a key role in the continuous quality control of asphalt production by measuring the viscosity of bitumen in the production stream in real time, without requiring manual sampling or interrupting the production process. Historically, the quality of oxidized asphalt and the determination of the end point of production were assessed by measuring “penetration” or using the “softening point” ASTM methods.

This continuous monitoring makes it possible to immediately detect any deviations in temperature or composition that could affect the product’s rheological properties, thereby ensuring consistent homogeneity across batches. A major advantage is the reduction of risks associated with handling or sampling of high temperature Asphalts.

Conclusion

In bitumen blowing, the quality of the final product depends on stopping the reaction at exactly the right moment. Inline viscosity measurement, correlated with softening point and penetration, turns that decision into a real-time, data-driven step. The result: consistent grades, fewer hot samples and better control of blowing time.

Our service & support team can assist you with installation and with setting up the correlation on your products.

Want to control the end point of your bitumen blowing in real time? Contact our viscometry experts to discuss your process.

If you have any questions, please fill in the form.